aboutcorrosion.com
Pre-exposure embrittlement and stress corrosion cracking of magnesium alloy AZ31B in chloride solutions – Publication | About Corrosion
In this manuscript, we investigate the influence of hydrogen on the environmentally assisted cracking and pre-exposure embrittlement of alloy AZ31B.‚Äč